Thermal Properties
Thermal Conductivity |
1.38(W/m°K) |
Coefficient Of t\Thermal Expansion(0~1000°C) |
0.55(10-6/°C) |
Normal Operating Temperature |
Continuous Usage |
~1050°C |
Non Continuous Usage |
~1250°C |
Strain Point |
~1075°C |
Annealing Point |
~1180°C |
Hot Pressing Temperature |
~1700°C – 2100°C |
Devitrification Temperature |
Starting at ~1000° C. high temperature accelerates Devitrification, especially with surface contaminants such as alkaline solution, salts and vapors. |
Physical Properties
|
Units of Measure |
Value |
Density |
gm/cc (lb/ft3) |
2.2 |
Porosity |
%(%) |
0 |
Tensible Strength |
106 Pa |
48.3 |
Young’s Modulus |
106 Pa |
71.7 |
Hardness |
Kg/mm2 |
600 |
Thermal Conductivity |
W/m°K |
1.38 |
Coefficient of Thermal Expansion |
10-6/°C |
0.55 |
Specific Heat |
J/Kg.°K |
740 |
Dieletric Strength |
Ac-kv/mm (volts/mil) |
30 |
Dieletric Constant |
@1MHz |
3.82 |
Index of refraction @ 587.6nm |
— |
1.4585 |
Fused Quartz Average Transmission Curve
Includes Surface Reflection Losses